The main components are nano-silica aerogel, high-performance elastic emulsion, water solvent, etc. Applied to the existing and new building interior and exterior wall thermal insulation coating, this product can play a very good thermal insulation effect, aerogel coating system can prevent the outside heat into the room, reduce the energy consumption of air conditioning. In the cold winter, prevent the indoor heat to the outdoor diffusion, reduce the use of heating or air conditioning energy consumption, to warm in winter and cool in summer.

 

Test Items Unit Data
Appearance Status white paste
Construction method Scraping, wiping and spraying
Specifications Barrel 12 Kg
coefficient of thermal conductivity W/(m · K) 0.035
Specific Gravity kg/L 0.6
dry density Kg/m3 200
Construction temperature ≥ 5
dry film thickness mm ≥ 2
Material amount kg/m2 1(2mm thickness)
Drying time h 6(2mm thickness, surface dry)

 